HydroFix Damp-Proofing Plaster
In a standard application, a single coat 2-3 mm thick is sufficient. In cases of very severe damp, 2 coats can be applied. Before the second coat, the first coat must be allowed to dry completely (at least 6-8 hours, ideally 24 hours). The second coat is applied in the opposite direction.